- BrandКонстантиновский завод неформованных огнеупоров
- Country of manufactureUkraine
- Weight20 kg
- TypeThe mixture
The mixture for masonry fireplaces and stoves to be used during preparation (pre) work for laying so - called refractory bricks. Proper use of the customer purchased products will help facilitate the implementation of tasks and reduce the time of the work itself. The solution for masonry oven can be bought on the web page of our company by selecting the appropriate section and goods from the proposed list. A mixture of masonry stoves and fireplaces, the price of which is set quite low, it has several important advantages for the consumer, including significant can be considered:
• Adhesion fast, which allows technicians to quickly begin substantive work as scheduled and ready to hand over the project;
• high strength, which is important for the duration of service of the furnace, the fireplace or barbecue;
• a sufficiently high temperature operation of the product, which provides the necessary freedom of action to builders;
• product perfectly lends itself to mixing.
All information, prices of products, all kinds of contacts and a list of all the services provided can be found on the company's website.
MAIN FACTORS | |
Maximum operating temperature is 0 ° C | 1200 |
Material consumption at the brick masonry 1 / kg, the seam 4 mm | 0.45 - 0.5 |
seam thickness, mm | 4 - 12 |
The addition of water when used, L / 20kg dry mixture | 5 - 5,5 |
Mixing | Drill Mixer |
The drying temperature 5 - 200S | up to 2 weeks |
PERFORMANCE OF WORK
Before starting work, brick surface clean from dust, dirt and moisturize, dropping a brick in the water at 10 - 15C. It is not recommended to use brick with a paint and traces of soot.
Mixing and brickwork recommended at temperatures below 5 0C.
The container is filled with powder and water is added.
The mixing time to obtain a homogeneous mixture of at least 5 minutes.
In the case of repairs work surface is cleaned to a depth of 3 - 5 cm, with a dusting brush in mezhkirpichnom space. Stripped seam well - moistened with a brush. Prepared solution is applied to completely fill the seam is overwritten.
Duration of use of the finished mixture to 60 minutes with additional stirring.
Total exposure time of the end of laying at least 2 weeks.
Shelf life: | 12 months in a dry place |
Packaging: | Мешок бумажный весом 20к |