Technical characteristics
  • BrandЗавод КазОгнеУпор
  • Country of manufactureKazakhstan
Description
Scope:

Production of blocks, products and monolithic concrete lining with the lowered heat conductivity for thermal, chemical and metallurgical units.

Brand Name and characteristic of mix
SKB-94 Mix corundum concrete with a mass fraction of oxide of aluminum not less than 94%
SKBT-1,6 Mix corundum concrete heat-insulating with the seeming density no more than 1,6 g/cm3
SMKBT Mix mullitokorundovy concrete heat-resistant
SMKB-90 Mix mullitokorundovy concrete with a mass fraction of oxide of aluminum not less than 90%
SMKB-85 Mix mullitokorundovy concrete with a mass fraction of oxide of aluminum not less than 85%
SMKB-80 Mix mullitokorundovy concrete with a mass fraction of oxide of aluminum not less than 80%
SMKB-72 Mix mullitokorundovy concrete with a mass fraction of oxide of aluminum not less than 72%
SMKB-65 Mix mullitokorundovy concrete with a mass fraction of oxide of aluminum not less than 65%
SMKRB-50 Mix mullitokremnezemisty concrete with a mass fraction of oxide of aluminum not less than 50%
SSHB - 40 Mix shamotny concrete with a mass fraction of oxide of aluminum not less than 40%

Physical and chemical indicators

Name of an indicator Value for brand
SKB-94 SKBT-1,6 SMKBT SMKB-90 SMKB-85 SMKB-80 SMKB-72 SMKB-65 SMKRB-50 SSHB-40
Mass fraction, %:
AI2O3, not less 94 90 90 90 85 80 72 65 50 40
SAO, in limits 2,5-4,0 ≤7,5 2,5-4,0 2,5-4,0 2,5-4,0 2,5-4,0 2,5-4,0 4,0-6,0 4,0-6,0 4,0-6,0
Mass fraction of moisture, %, ≤0,3 ≤0,3 ≤0,3 ≤0,3 ≤0,5 ≤0,5 ≤0,5 ≤0,5 ≤0,8 ≤0,8
Fire resistance about With, not below 1770 1670 1750 1750 1750 1730 1730 1710 1690 1670
The seeming density, g/cm3 - ≤1,6 - - - - - - - -
Strength on compression after heating to 110 ° C, N/mm2 - 10 - - - - - - - -

Grain structure for brands

Pass through grids, %, SKB-94 SKBT-1,6 SMKBT SMKB-90 SMKB-85 SMKB-80 SMKB-72 SMKB-65 SMKRB-50 SSHB-40
No. 8, not less 95 - 95 95 95 95 95 95 95 95
No. 5, not less - 95 - - - - - - - -
No. 3,2, no more 80 - 80 80 80 80 80 80 80 80
No. 05, no more 55 - 55 55 55 55 55 55 55 55
No. 0063, in limits 30-40 - 30-40 30-40 30-40 30-40 30-40 30-40 30-40 30-40